Dear Gary,

It is possible the mask was not fully cured or properly exposed? Check to
see what the actual exposure energy was? Ask the supplier to enact an
additional UV bump or thermal cure to see if this helps.

Good luck,

Mike Carano

        -----Original Message-----
        From:   Gary Camac [SMTP:[log in to unmask]]
        Sent:   Monday, January 10, 2000 9:00 AM
        To:     [log in to unmask]
        Subject:        [TN] Residue on assemblies after cleaning

        Good morning everyone,

        We are seeing a film on some circuit board assemblies after
        a pass through our in-line cleaner.

        We are using an RA flux and a soaponifier in the cleaner.
        The film is only showing up on boards that have a high gloss
        LPI mask.
        Multiple passes through the cleaner will not remove the
        film.
        The film can be easily wiped off with a dry wipe.
        The film can be cleaned off brushing with isopropyl alcohol
        The pattern of the film is an image of the flux residue that
        was on the board prior to cleaning.

        Any ideas as to what is going on.

        Thanks in Advance,
        Gary Camac

        ##############################################################
        TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
        ##############################################################
        To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
        the body:
        To subscribe:   SUBSCRIBE TECHNET <your full name>
        To unsubscribe:   SIGNOFF TECHNET
        ##############################################################
        Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
        information.
        If you need assistance - contact Gayatri Sardeshpande at
[log in to unmask] or
        847-509-9700 ext.5365
        ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2