In a message dated 01/19/2000 4:45:20 PM Central Standard Time,
[log in to unmask] writes:
<< Hi Steve -
IBased on my experience with them, I think you'll do fine with your
micro-buggahs. Be sure that you have a steady, rumble free conveyor in your
oven. I know YOU know better than to have the design folks put mirror image
but for uninformed Technetters, such placement impedes accurate x-ray
inpection. Let us know how you make out.
Regards,
Phil Zarrow
ITM, Inc.
Durham, NH USA
www.ITM-SMT.com >>
Hi Phil!
Thanks! There's only 1 µBGA per board so that won't happen, but in a panel
like I was talking about they'll be on both sides of the panel....
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|