Nancy,
What is the construction of your flex? Adhesive or adhesiveless? If it is
adhesive type (acrylic), you may want to use mild solvent...Make sure the
solvent you are using is compatible with acrylic...
jk
At 12:21 PM 1/4/00 -0500, you wrote:
>TechNet,
>
> What is the best technique to clean flux off of a polyimide flex circuit
>after population? Thus far, we have been cleaning the flex circuits with
>alcohol but it is time consuming and tedious. We use a machine to clean
>rigid boards, but I am hesitant to use it for our flex circuits. How are
>you all cleaning your soldered flexible printed circuit boards.
>
> Thanks,
> Nancy
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|