Goh, check archives on my previous reply on this motto :
with this temps ; see if you could web the mask ;
as it's obvious the CTE's @ that fast temp shifts do fight (>large area
copper).
webbing gives you additional adhesion preventing the blisters .
Worked for me in past , check undercure as well (= instill some fear in fab
folks).
With one off case ; cure it could indeed be .
By the way would/could you have thermal relieve on your pads ?
and work on a hot plate (150'C) if feasible (or localised hot jet air)
pk
-----Original Message-----
From: Goh Guan Chye [mailto:[log in to unmask]]
Sent: Monday, 31 January 2000 20:28
To: [log in to unmask]
Subject: [TN] Measling after soldering
Hi ! Technetters,
May anyone advise a measling problem after manual soldering.
We have a batch of PCBA spotted with measling after manual soldering.
These measling happen surround the areas with large copper plane. This
is a 14-layer design (2.9mm thick) with 6 layers of large copper areas
(not full plane). Due to heat sinking problem, we use solder temperature
of 350 degC and the soldering duration is about 2-3 secs. To analyse on
the problem, we wave the assembly at solder bath temp of 250 degC, no
measling found.
The question now is, this is not the first time that we manual solder
high layer count MLB with large copper plane. We did not find any
measling problem. In such case, what could it be due to ? The bare board
quality problem ? Should the bare board must be able to withstand the
manual soldering that we used ?
If the measling doesn't meet the IPC acceptance criteria, would it
affect the bare board's reliability ?
Thanks for your attention and have a nice day.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|