What is the thickness of the panels you intend to plate? Hole size? Any
microvias? Pulse or DC? Air or Airless?
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Wayne Martin
Sent: Friday, January 28, 2000 1:18 PM
To: [log in to unmask]
Subject: [TN] Copper baths
Looking for resources on what is a good acid copper bath. Who is the
supplier and what is the name of the bath. Any help would be appreciated.
Wayne Martin
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################