Hello Ken,
IEC 60112 may be of help. It refers to the Comparative Tracking Index (CTI)
of boards.
Phil.
At 17:03 12/01/00 GMT, you wrote:
> Technetters,
>
> Could anyone tell me whether there is any international standards
> describing voltage required and other conditions to test for the
> isolation and insulation between tracks of different spacings on a
> printed circuit board without component inserted on it.
>
> Regards,
> KenF, jan 12,00
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
>the body:
>To subscribe: SUBSCRIBE TECHNET <your full name>
>To unsubscribe: SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>
Phil Dutton C.I.D.
Senior CAD Technician
IPC Certified Interconnect Designer
Vision Abell Pty Ltd
Second Avenue, Technology Park,
Mawson Lakes. SOUTH AUSTRALIA 5095
===============================================================
Phone : (08) 8300 4400 (reception)
Fax : (08) 8349 7420
email: [log in to unmask]
Internet Page: http://www.vsl.com.au
===============================================================
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|