TECHNET Archives

January 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="iso-8859-1"
Sender:
Subject:
From:
Paul Klasek <[log in to unmask]>
Date:
Fri, 28 Jan 2000 09:02:35 +1100
MIME-Version:
1.0
X-To:
"Collins, Graham" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Paul Klasek <[log in to unmask]>
Parts/Attachments:
text/plain (75 lines)
True Graham ; ages ago i cut a circle, hooked on a dozen washers and played
with degrees, points of entry, etc.,
(called validations, qualifications, etc.)
And yes, you get relatively individual results tied with individual designs
on individual boards .
Dead easy , give it a shot, nothing like seeing to believe or not, on Your
cards .

Eventually , ads-up all sums/cons/pros it's better to avoid (as you know)
wave .
Disparity of precise reflow profiles versus wave vertical steps technical
hypocrisy always amused me .
But we all do what we have to ...., just some caps really dislike it

happy navigations               paul

-----Original Message-----
From: Collins, Graham [mailto:[log in to unmask]]
Sent: Friday, 28 January 2000 4:45
To: [log in to unmask]
Subject: [TN] wave soldering - board rotation


Is the TechNet back up?  Yippee!

Good day TechNet!
Has anyone out in wave soldering land tried using a wave soldering fixture
that allows you to change the rotation of the board so that the edge of the
board isn't parallel to the conveyor?

I'm told that rotating the board slightly (say 5 degrees - not 90 degrees!)
can reduce the
occurrence of solder skips on SMT chips (caps and resistors).  Any
experience out there to confirm or deny this?

Final note: the board design is not suitable for a paste reflow of the SMT
parts followed by use of a partial wave fixture.  Otherwise that would be my
#1 choice...

regards,

Graham Collins
Process Engineer,
Litton Systems Canada, Atlantic Facility
(902) 873-2000 ext 6215

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2