Ralph
How high is "high"? I know Rogers makes some materials that get as high as
.6 to .8 W/m/K. That's relatively high compared to more conventional
laminate materials, but I don't think you're going to get a lot of heat out
through the laminate.
Mike McMaster
RF Product Engineer
Merix Corporation
503-992-4263
----------
From: Ralph Garvin [SMTP:[log in to unmask]]
Sent: Monday, January 24, 2000 1:26 PM
To: [log in to unmask]
Subject: Re: [TN] PCB SUBSTRATE MATERIAL;
attn: ALL
I have a question regarding pcb laminate materials. We are looking
for a material with a high thermal conductivity.
If there is anyone out there with knowledge of such or links to
same, it would be appreciated.
Thanks in advance.
Ralph Garvin
New Product Development
Westport Research, Inc.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Gayatri Sardeshpande at
[log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|