TECHNET Archives

January 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Carey Pico <[log in to unmask]>
Date:
Wed, 5 Jan 2000 09:55:48 -0500
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Nancy M. H. Holloway" <[log in to unmask]>
Subject:
From:
"Nancy M. H. Holloway" <[log in to unmask]>
In-Reply-To:
<004501bf5713$9052bdc0$4e84bece@pico>
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (138 lines)
To all,

   Nothing makes a beautiful joint like flux!  I have to admit, that during
my high reliability soldering training,  we were discouraged against using
flux when soldering, but it makes all the difference in world as to how
well the solder wets and flows.

                                Nancy

At 04:26 PM 1/4/00 -0800, Carey Pico wrote:
>To all
>
>I've been keeping out of this discussion.  But one thing I don't get... why
>isn't the board industry looking at a fluxless process?
>
>Carey
>
>-----Original Message-----
>From: Kelly M. Schriver <[log in to unmask]>
>To: [log in to unmask] <[log in to unmask]>
>Date: Tuesday, January 04, 2000 2:52 PM
>Subject: Re: [TN] cleaning flex circuits
>
>
>>Hi Nancy -
>>
>>To begin with, the cleaning media is driven by the particular flux you are
>>using.  This, in turn, will drive the issue of what equipment you may be
>>able to use for the process.  I have had good success removing RMA residues
>>from flex circuits with quite a number of blended solvents in vapor
>>degreasers and conveyorized spray systems.  Size of the flex assembly must
>>obviously be considered - there are a number of suppliers who can provide
>>cleaning baskets to restrain small flexes for processing thru conveyorized
>>cleaning systems.  Manual cleaning would not be my first choice if I were
>>dealing with a high reliability article, particularly if it were to be
>>conformal coated.
>>
>>Another possibility might be one of the saponifiers, in either a heated
>bath
>>or a "dishwasher"  type system.
>>
>>If you are not currently using a low residue ("no clean") flux, might that
>>be a possibility?  If this is a consideration, and you plan to conformal
>>coat or use adhesives on the assembly, be sure to verify full compatibility
>>of the flux residues and the specific coating material you intend to use
>>before proceeding.
>>
>>Contact me directly if I can be of assistance.
>>
>>Regards - Kelly
>>
>>
>>
>>
>>-----Original Message-----
>>From: Nancy M. H. Holloway <[log in to unmask]>
>>To: [log in to unmask] <[log in to unmask]>
>>Date: Tuesday, January 04, 2000 10:57 AM
>>Subject: [TN] cleaning flex circuits
>>
>>
>>>TechNet,
>>>
>>>   What is the best technique to clean flux off of a polyimide flex
>circuit
>>>after population?  Thus far, we have been cleaning the flex circuits with
>>>alcohol but it is time consuming and tedious.  We use a machine to clean
>>>rigid boards, but I am hesitant to use it for our flex circuits.  How are
>>>you all cleaning your soldered flexible printed circuit boards.
>>>
>>>                                Thanks,
>>>                                Nancy
>>>
>>>##############################################################
>>>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>>>##############################################################
>>>To subscribe/unsubscribe, send a message to [log in to unmask] with
>following
>>text in
>>>the body:
>>>To subscribe:   SUBSCRIBE TECHNET <your full name>
>>>To unsubscribe:   SIGNOFF TECHNET
>>>##############################################################
>>>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>>additional
>>>information.
>>>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>>>847-509-9700 ext.5365
>>>##############################################################
>>
>>##############################################################
>>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>>##############################################################
>>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in
>>the body:
>>To subscribe:   SUBSCRIBE TECHNET <your full name>
>>To unsubscribe:   SIGNOFF TECHNET
>>##############################################################
>>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
>additional
>>information.
>>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>>847-509-9700 ext.5365
>>##############################################################
>>
>
>##############################################################
>TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
>##############################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
>the body:
>To subscribe:   SUBSCRIBE TECHNET <your full name>
>To unsubscribe:   SIGNOFF TECHNET
>##############################################################
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information.
>If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
>847-509-9700 ext.5365
>##############################################################
>
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2