Steve,
My concern is related with board warpage inside reflow oven. Depending on
your panelization size and type ( v-score or tabs )you can induce more
warpage that can affect BGA to board contact. But you can put a wire inside
the oven ( front to end ) to avoid warpage in the same way that is used at
solder wave machine.
Thanks
Jorge Dourado de Santana
Maintenance / Process Engr
Microtec - Brazil
> -----Original Message-----
> From: Stephen R. Gregory [SMTP:[log in to unmask]]
> Sent: 19 de Janeiro de 2000 18:40
> To: [log in to unmask]
> Subject: [TN] [TN] Double-sided reflow with µBGA...
>
> Hi-dee ho ya'll!
>
> Gotta question, I gotta a lil' board here (.68" X 4.18") that is
> double-sided
> (all SMT no through-hole) and has a 256-ball µBGA on one side. It's a
> prototype right now (we're only building 5 or 10 assemblies).
>
> In my panelization recommendations I was thinking of having the panel made
>
> with the boards alternating top/bottom/top/bottom etc., that way I would
> only
> need one stencil, and we would only have to do one machine set-up when
> building the panels, because we would be building both the top and bottom
> at
> the same time. Once one side of the panel is built, you just take it from
> the
> reflow oven and put it back into the printer to do the second side of the
> panel, but you wouldn't have to change a thing on the printer or pick and
> place machines because the bottom of the panel is an exact mirror of the
> top...follow me?
>
> Anyways, my real question is about double-sided reflow of the µBGA, I know
>
> the surface tension will be there to hold the part, but I've never done it
>
> before and don't know for sure if there will be any problems...I wouldn't
> think so, but I though I'd ask ya'll to see if any of you have ever done
> it,
> and if there were any problems.
>
> Thanks ya'll!
>
> -Steve Gregory-
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|