Pete, the range is a bit tight on the top side, and if you call out a nominal on the
bottom than give me a plus and minus please. 200 micro inches plus or minus 100 micro
inches could be reasonable. Its a bit of a rookie call out. Everything depends on the
geometry and uniformity of the features. Or, perhaps through experience the customer
has found this near actual thickness from previous vendors? Its been my experience
that almost no one understands the nuances of the process, and specs for HASL ends up
being an exercise in rear end covering, in case of solderability problems, eh?
Mark Simmons, V-Score Central, Inc.
Pete Nemcik wrote:
> Hi Techneters,
> quoting from a print: "FINISH: CONDUCTOR PATTERNS ON FINISHED BOARD
> SHALL BE SOLDER COATED PER IPC-D-275 AND HOT AIR LEVELED (HASL) TO A
> FINAL THICKNESS OF .0001-.00025 LAYER 1 (TOP), .00025 NOMINAL LAYER 2
> (BOTTOM)."
> Is this realistic? Can anybody do this? Any help and advice is
> appreciated. Any companies capable of doing, please me contact directly.
>
> Thanks!
>
> Peter Nemcik
> Modular Components National Inc.
> Forest Hill, MD 21050
> (410) 879-6553
> FAX (410) 838-7629
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|