TECHNET Archives

January 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 19 Jan 2000 11:14:57 EST
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
From:
"Stephen R. Gregory" <[log in to unmask]>
Parts/Attachments:
text/plain (38 lines)
In a message dated 01/19/2000 9:55:42 AM Central Standard Time,
[log in to unmask] writes:

<< Ok..so what are the causes of solder beads?? >>

Hi Jan!

Solder beads or "Squeeze balls" as they're sometimes referred to, are caused
by too much of the gray stuff...solder paste. In a cleaning environment
they're usually not a problem because they wash off. But in a no-clean
environment, BIG headache!

They can be eliminated by modifying the apertures in your stencil to reduce
the volume of paste you're putting down. Instead of square apertures you can
turn them into triangles or "homeplates" with the pointy ends pointing
towards each other to the center of the footprint. A lot of  stencil vendors
will do this automatically...at least mine does. I just tell them I want
no-clean apertures for all the passives...I think it's an extra $25-50 charge
for the editing they have to do in the gerber.

Hope this helps...

-Steve Gregory-

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2