We use Axarel 2200 or Isopropyl alcohol, acid brush (carefully) and vacuum
away residue. Yes, time consuming, but we don't have that many. I would
imagine large quantities could be cleaned in a batch washer with proper
fixturing to keep small flex circuits from getting blown off the rack or
being flexed too much.
R. G. Blomberg
Honeywell -SASSO
Staff Production Engineer
-----Original Message-----
From: Nancy M. H. Holloway [mailto:[log in to unmask]]
Sent: Tuesday, January 04, 2000 12:21 PM
To: [log in to unmask]
Subject: [TN] cleaning flex circuits
TechNet,
What is the best technique to clean flux off of a polyimide flex circuit
after population? Thus far, we have been cleaning the flex circuits with
alcohol but it is time consuming and tedious. We use a machine to clean
rigid boards, but I am hesitant to use it for our flex circuits. How are
you all cleaning your soldered flexible printed circuit boards.
Thanks,
Nancy
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|