TECHNET Archives

January 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Ryan Grant <[log in to unmask]>
Date:
Tue, 4 Jan 2000 06:40:08 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Ryan Grant <[log in to unmask]>
Parts/Attachments:
text/plain (86 lines)
Hi Tana,
        "Abandon time" is the same as the more common term "stencil life"
and is sometimes called "lunch time".

        When I first got hired into this industry, since I knew nothing, I
figured a trip to the local library would do me good.  After reading a half
a dozen books on the topic, I became very frustrated that none of the books
would give me specifics (typical stencil lives, reflow profiles, washer
nozzle pressures, etc.).  They all said the process had to be "optimized".
So the answer to you question is "it depends".

        It depends on the solder paste manufacture
        It depends on the local relative humidity
        It depends on the aperture opening sizes
        The list continues

        At one time we used a paste that had a stencil life of 10 minutes
when using 16mil fine pitch and the RH is 20%.  We now use a paste that
performs great after sitting unused on the stencil for 2 hours; even on fine
pitch.

        Sorry for the long answer, so to give you a generic short answer;
put the paste back into the jar if it will be unused for an hour or more on
non fine pitch.  For fine pitch, the paste should be kneaded before printing
if the paste sits for 20 minutes or more.

        For driving really low DPMO values for solder defects, many of us
like to get really anal and require kneading of the paste if it sits for
more than 6 minutes.  (I can't wait to get in a rheometric head).

        Kneading paste on very large boards must be done by printing a board
and then scraping and washing the paste off it.

> -----Original Message-----
> From: tn [SMTP:[log in to unmask]]
> Sent: Tuesday, January 04, 2000 4:00 AM
> To:   [log in to unmask]
> Subject:      [TN] Solder Paste "Abandon Time" and "Stencil Life"
>
> Dear TechNetters,
>
> Happy New Year to you all.
>
> I would like to know what "abandon time" is normally used in the
> industry with solder paste stencil printing [1, 2, 4, 8, 10, 14+
> Hours]. Your response will be highly appreciated.
>
> Regards
> Tana
> PS: I have heard of stencil life, are these synonymous?
> Dr. Tennyson Nguty, Electronics Manufacturing Research Group,
> AeroMech Department, Newton Building, Salford University
> Manchester M5 4WT, UK. Tel: 0161-295 5951/4696, Fax: 0161-295 5575/5108
> Email: [log in to unmask]
> >> If you want to make your dreams come true, wake up!
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2