Good idea. A flexible conductive epoxy of the type supplied by the regular adhesive
suppliers (who are probably going to be looking at bendy versions of their die attach
products) is worth a go provided you can get a cure schedule which is compatible
with the flex circuit material (and not effect adhesion of the foil), but may not be the
best/sole option. For example how are you going to maintain your outline when laminating
this stuff into the middle of a flex circuit, if uncured, or get adhesion if cured on one
layer? Assuming I read you right.
So it might be a good idea to try also suppliers of inks and things for flex circuits, I
think Acheson is a leader here. They anyway will be uptospeed on what can can't be done
and how to.
There are companies that specialise in RF shielding products, problem is I am not familiar
with your market place.
Finally when all else fails they say RTFM [read the manual]. In this case a Nepcon West
Show Catalogue. This should give you classified lists of companies in the unlikely event
that Technet strikes out (if that's the correct phrase).
Best of luck
Mike
----- Original Message -----
From: <[log in to unmask]>
To: Michael Fenner <[log in to unmask]>
Sent: 13 January 2000 12:28
Subject: Re: [TN] Flexable conductive epoxy
>
>
> Mike,
> Thanks for your response.
> What we're trying to achieve here is an EMI shield at the ends of a flex
> circuit.
> Imagine an outline that resembles a ginger bread man (no kidding).
> I'm trying one option of using a flexible conductive type epoxy to achieve total
> shielding between the layer edges and in between the flex layer themselves.
> I realise that what I'm asking for may not be attainable with the parameters
> outlined, NASA approved little or no outgassing, no particulates and able to
> withstand a sustained space environment.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|