Ted
We have been switched to TFT about 6 months.
10%-15% Speed increase and consumption decrease.
PRINT&ETCH capability is dependent on chemical and machine characteristics,
with the latter being much harder to control.
We have had no glitches and don't know of any negatives.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Ted Wiktorowicz
Sent: Wednesday, January 12, 2000 7:50 AM
To: [log in to unmask]
Subject: [TN]
Because I have not recieved any response, I am trying to re-send an earlier
request in regards to Thiourea free alkaline etchant.
If anyone has had any experience with it I would very much appreciate any
feed back.
- has the claimed benefits (less undercut, higher etching rates, less
attack on print & etch resists) been realized?
- do you see a lower consumption of TFT etchant in comparison with your old
alkaline etchant - if so can you guesstimate a percentage?
- is the switch over fairly easy?
- are there any negatives to switching?
Thanks in advance for your help
Ted
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|