James LIU Chunguang <[log in to unmask]>
Reply To:
Asia Committe Task Group Forum <[log in to unmask]>, James LIU Chunguang <[log in to unmask]>
Date:
Mon, 18 Apr 2011 03:53:48 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (1 lines)
请见下面回答。



Best Regards,



NEW:2011年5月 苏州

           第二届IPC手工焊接竞赛-华东赛区期待您的参与!

James Liu 刘春光

Director, Industry Programs培训中心主任/工业项目总监

IPC China

[cid:[log in to unmask]]



北京市经济技术开发区宏达北路18号大地国际大厦407A

Room 407A,Dadi international Building, #18 Hongda North Rd., BDA 100176 Beijing China

Tel:   +86 10 67885326

Fax:  +86 10 67885326

MP:   +86 136 0133 3491

[log in to unmask]<mailto:[log in to unmask]>

www.ipc.org.cn<http://www.ipc.org.cn/>



发件人: TGAsia [mailto:[log in to unmask]] 代表 Shijun_Tang (b 唐仕俊)

发送时间: 2011年4月18日 16:22

收件人: TGAsia

主题: [TGAsia] 焊錫研究中的名詞理解.



各位大俠

    焊錫研究中有以下名詞不知怎樣理解是正確的,請賜教.

1.      熔點固相線 (刘春光:这是金属材料相图的一条线:低于这条线,物质呈固态。)

2.      熔點液相線.(刘春光:与上相同:高于这条线物质呈液态。)

3.      引張強度.(刘春光:这可能是台湾叫法,不知道大陆对应的名词,在此不好妄加推断)

4.      延伸率(刘春光:物质发生延伸形变时的最大形变率)

5.      線膨脹系數(刘春光:物质在一个方向上的热胀系数)

6.      擴散率(刘春光:可能是台湾叫法,对应的大陆叫法是否是铺展率?)

Thanks!

祝:身體健康,工作愉快.

康舒科技(東莞)有限公司

IE:唐仕俊

TEL:(0769)8791-5950 Ext:36902



______________________________________________________________________

This email has been scanned by the MessageLabs Email Security System.

For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>

______________________________________________________________________


ATOM RSS1 RSS2