I agree, except pads that are big enough to provide fillets on the side have
been known to cause skewing, no?
James
> From [log in to unmask] Wed Jun 11 05:01:45 1997
> Resent-Date: Wed, 11 Jun 1997 07:05:22 -0400 (EDT)
> Resent-Sender: [log in to unmask]
> Old-Return-Path: <[log in to unmask]>
> From: [log in to unmask]
> Date: Wed, 11 Jun 1997 07:05:22 -0400 (EDT)
> To: [log in to unmask]
> Subject: Re: ASSY: Are U Square or Round or Oval
> Resent-Message-Id: <"ORKAP3.0.cIB.CGedp"@ipc>
> Resent-From: [log in to unmask]
> X-Mailing-List: <[log in to unmask]> archive/latest/13294
> X-Loop: [log in to unmask]
> Resent-Sender: [log in to unmask]
> Content-Length: 1685
>
> Hi John,
> The reason tombstoning occurs at all is that the outer edges of the pads
> protrude too much beyond the chip components--if you have no large solder
> fillets you will not get tombstoning because the required surface tension
> forces that cause tombstoning exist only with large fillets and unsymmetric
> position. In reflow soldering these components there is really no need for
> protruding pads (to be touched by the wave) and the resulting fillets at all.
> These components are so small, that certainly there is no need for fillets
> for reliability reasons.
> Some people also found success with narrower pads which diminish fillet size,
> but the best way is to have pads that essentially are only underneath the
> components-- if you really want fillets put them to the side of the
> components.
>
> Werner Engelmaier
> Engelmaier Associates, Inc.
> Electronic Packaging, Interconnection and Reliability Consulting
> 23 Gunther Street
> Mendham, NJ 07945 USA
> Phone & Fax: 973-543-2747
> E-mail: [log in to unmask]
>
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To subscribe/unsubscribe send a message <to: [log in to unmask]> *
> * with <subject: subscribe/unsubscribe> and no text in the body. *
> ***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
> ***************************************************************************
>
>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|