Hello,
Once again we're seeking a source of FR-4 laminate with no UV block
added to the resin. Also know as "white laminate," we need this
laminate to be almost UV transparent. Since most of the laminators
consider this product to be obsolete, we find increasing difficulty
in locating a source. We do not need a sufficient quantity to
justify a dedicated treater run of the FR-4 prepreg but if anyone
knows where we can by any thin core half ounce or one ounce single
or double sided laminate with no UV block we would appreciate the
advise.
Thanks,
Dan Brandler
Ohmega technologies, Inc.
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|