Phil,
Underfills that require solvent removal to cure will just take time for the underfill solvent to migrate out from under the package... A quick and dirty way to figure the cure time would be to check the cure time for a thick section of the underfill...
Try casting a block the thickness of the 1/2 the BGA with tape on the bottom... Then you can peel off the bottom tape in sections after certain durations, checking the bottom face if the material has sufficiently cured...
Oh... Merry Christmas...
Paul
Paul Edwards
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Phillip Bavaro
Sent: Wednesday, December 24, 2008 11:17 AM
To: [log in to unmask]
Subject: Re: [TN] Underfill, inhibition due to leftover activators in the flux residue
Thanks Wayne.
I will do a little experimentation to see if I can recreate the problem in
a lab environment.
When you misted the sample, were you talking about an underfilled BGA or
just raw underfill material?
Phil
At 12:43 PM 12/23/2008 -0500, Thayer, Wayne wrote:
>I have been in underfill "hell" numerous times.
>
>I still don't have a complete understanding of what makes it decide to not
>cure properly, but moisture can be a big problem, as far as some of the
>Henkel products go. We are getting better results with extended bake
>cycles to eliminate any moisture from the assembly. This might have
>something to do with your problem too: Send it through the oven a number
>of times, and each time it will be a bit drier.
>
>I use mostly RMA flux and solvent clean. I have mixed raw RMA flux
>directly with the underfills we use and they seem to cure OK. Only way I
>could get the uncured goo witnessed sometimes on the production line was
>to literaly mist it with water prior to attempting to cure.
>
>Good Luck!
>
>Wayne Thayer
>
>-----Original Message-----
>From: TechNet [mailto:[log in to unmask]] On Behalf Of Dwight Mattix
>Sent: Tuesday, December 23, 2008 11:46 AM
>To: [log in to unmask]
>Subject: Re: [TN] Underfill, inhibition due to leftover activators in the
>flux residue
>
>At 04:54 AM 12/23/2008, David D. Hillman wrote:
> >But - if you have a BGA that is sufficiently large and has significant
> >I/O, you are going to have some flux residue remaining under the
> >component.
>
>/heh no kidding.
>
>Phil,
>This under a 7xxx series MSM? Almost 700 pins on a .5mm or .4mm package?
>
>You're going to love the the 8xxx series. :-) lol!
>
>Merry Christmas,
>dw
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
>unsubscribe, send a message to [log in to unmask] with following text in the
>BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
>(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
>Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts:
>send e-mail to [log in to unmask]: SET Technet Digest Search the archives of
>previous posts at: http://listserv.ipc.org/archives Please visit IPC web
>site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
>ext.2815
>-----------------------------------------------------
>
>This e-mail and any files transmitted with it may be proprietary and are
>intended solely for the use of the individual or entity to whom they are
>addressed. If you have received this e-mail in error please notify the sender.
>Please note that any views or opinions presented in this e-mail are solely
>those of the author and do not necessarily represent those of ITT
>Corporation. The recipient should check this e-mail and any attachments
>for the presence of viruses. ITT accepts no liability for any damage
>caused by any virus transmitted by this e-mail.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
==============================================================================
This email and any attachments thereto may contain private, confidential, and
privileged material for the sole use of the intended recipient. Any review, copying,
or distribution of this email (or any attachments thereto) by others is strictly prohibited.
If you are not the intended recipient, please contact [log in to unmask]
immediately and permanently delete the original and any copies of this email and
any attachments thereto.
==============================================================================
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|