Hi Bob:
You might have to hand solder it. Preheat board, place
it over a hot plate to maintain temp and using a hot tip, place tip
mostly against the lead and also touch the pad. Use plenty of flux, you
will get close to 100% fill. We developed this procedure on a board that
had every other layer including top and bottom, a ground plane. All
components were metalized and flush to the board, plugging the barrels
at the component side. Assembly looked all silver color. It was a very
difficult board, still we had at least 60% fill.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, October 10, 2006 2:00 PM
To: [log in to unmask]
Subject: Re: [TN] vertical fill problem
Hi Bob,
Lot's of pre-heat, and pre-baking in an oven just immeadiately prior to
wave helps a lot with big, heavy, high thermal mass boards.
But if it's a class 2 assembly, the J-STD gives you an out under 6.3.2:
"As an exception to the Class 2 fill requirements in Table 6-5, for
plated through holes connected to thermal or conductor planes that act
as thermal heat sinks, a 50% vertical fill of solder is permitted, but
with solder extending 360-degrees around the lead with 100% wetting from
the barrel wall to lead on the secondary side, and surrounding PTH's
meeting requirements of Table 6-5."
-Steve Gregory-
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Arciolla
Sent: Tuesday, October 10, 2006 12:44 PM
To: [log in to unmask]
Subject: [TN] vertical fill problem
Good afternoon,
I have a situation where I have a transformer that I am populating in a
pcb and I have a ground plane right up next to it and between the ground
plane and the core of the transformer, I cannot meet the IPC requirement
of 75% vertical fill on the tranformer leads. Any suggestions?
Thanks in advance,
Bob Arciolla
Endicott Research Group
Quality/Safety Manager
607 754-9187 ex 3034
607 754-9255 fax
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
cell 607 624-8516
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|