SOLDER BALL PROBLEMS: ANOTHER CULPRIT TO CHECK THAT I HAVE NOT SEEN 
MENTIONED IS TO CHECK THE BULK SUPPLY OF FLUX FOR MOISTURE.
--------------------------------------