TECHNET Archives

August 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stephen R. Gregory" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 4 Aug 2000 22:16:00 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (50 lines)
In a message dated 8/4/00 4:34:26 PM EST, [log in to unmask] writes:

<< I would check out the Intel QX3 Computer Microscope, in fact I am surprised
 that I have not seen more of them at different shops.  They cost around $70
 to $75 and are a snap to hook up via USB.  Using a 15 inch monitor you can
 get 200x magnification.  The pictures that I have seen it capture (video
 too) are really great and at that price what can you loose?

 Check out http://www.intelplay.com/home.htm

 David >>

Hi David!

A guy at work here got one of the microscopes...I must admit it's pretty
cool, but not very practical in a electronics application. It's mostly for
microscopic slides. You run into throat depth problems when you have
something bigger than a slide.

Yeah, they say that you can remove it from the stage, and hand hold it for
images, but if you try and hold it in focus at 200X power to capture a image,
your heartbeat through your fingers will be a problem when trying to stay in
focus for a image capture. Also, from playing with the one that a fellow
worker brought here, anything higher than 100X it becomes very "pixel-lated"
in the image...that is; not very clear.

Not to say that isn't a cool toy, but not something that I would recommend as
a tool to create high-magnification digital images of printed circuit
assembly issues...

Maybe someone can come up with some way to use this thing, but as it's sold,
it's not a good tool...just my worthless opinion. But at $70.00 there ain't
much to lose.

-Steve Gregory-

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2