Good morning Techneters,
I am working on oven profiler consolidation project.
Currently, we have 540 Product Profile for each oven.
For 13 oven machine, we have 7020 profiles. That is
way too many for a memory manufacture!
We currently use water-soluble solder and no clean
solder. We know that for each product, the pre-heat
zone, soak-zone, re-flow zone, and temperature could
be a bit different from one Solder Paste Manufacture
to other, or from one Solder Paste type to others, or
even from single side, to double side.
HOWEVER, for memory, the width, length, thickness, and
number of ICs, resisters, capacitors, and others are
limited to a certain number, i.e, PCB height is less
than 1.7 inches; PCB thickness is equal or less than
0.05 inch; PCB length follow the spec. of 5.25” for
DIMM, DDR, RIMM, 2.66” for SODIMM, 4.25” for 72 Pin
SIMM, etc.
I have heard that out there, there is a way to reduce
from 1000s down to 10-100 oven profiles based on
Mass/Density. And of course, there are many other
scientific ways that I have not heard of. Please help
me! What would be the best method you recommend or you
have successfully tried to reduce the number of oven
profiles down to a control/reasonable numbers?
Your advice and suggestion are greatly appreciated.
Stacy
__________________________________________________
Do You Yahoo!?
Send FREE video emails in Yahoo! Mail!
http://promo.yahoo.com/videomail/
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|