Plasma is absolutely not dead and we process about 30% of FR4 requiring
positive etchback. We also use plasma for TPA, Polyimide, Getek, PTFE's
and several hybrid builds. New equipment is also available as the
technology is still in development and support.
Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
Voice - 802.257.4571 ext 21
Fax - 802.257.0011
<http://www.vtcircuits.com/>
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Wrobel, Clayton
Sent: Friday, October 27, 2006 8:39 AM
To: [log in to unmask]
Subject: [TN] Plasma Etch back and Desmear
We are primarily a military OEM and have specified Plasma Etch back of
0.0002 to 0.003". This was to support (the now defunct) Mil 5510. We
have had little or no problems with this requirement.
Fast forward: Our new CEM says that this is old technology and that
their suppliers no longer have the equipment to do plasma etch back.
They do not specify what they want to use for a desmear process. This
is a MAJOR CEM house so I am hesitant to tell them to "stuff it". (Pun
intended: It IS Friday)
So, the question: What is the industry standard for hi-rel/military
class 3 PCB's now? And is Plasma Etchback dead? I am very confused, as
I thought the trend was to MORE Plasma etchback, not less.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|