Ordinary paper is mostly cellulose which is sufficiently hygroscopic
with normal humidities (down to <20% RH) to not generate/retain an
electrostatic charge. Of course, electrical papers, such as used for
transformer interleaving, may have different characteristics.
I would be much more worried about coating mist particles with friction
against the air and the PCB!
Brian
- bogert wrote:
> July 10, 2008
>
> Unless the paper is conductive and the surface on which the paper rests
> is conductive and properly grounded, one should not rest any ESD
> sensitive PWA's on top of paper. Paper is normally considered an
> insulator, not a conductor and therefore this is a violation of the ESD
> S 20.20 document invoked via J-STD-001 which prohibits insulators from
> the work station unless it can be proven that they are not capable of
> producting damanaging ESD voltages.
>
>
>> From: "Kane, Amol (349)" <[log in to unmask]>
>> Reply-To: TechNet E-Mail Forum <[log in to unmask]>, "Kane,
>> Amol (349)" <[log in to unmask]>
>> To: [log in to unmask]
>> Subject: [TN] Conformal Coating Waste
>> Date: Wed, 2 Jul 2008 09:16:53 -0400
>>
>> Dear Technetters,
>> We regularly use absorbent paper to rest the boards in the conformal
>> coating booth as we spray them (UV cure coatings). A question came up
>> recently about the paper being hazardous waste due to uncured coating
>> on it. I want to know if:
>> 1. Anybody else is using a similar method to coat the boards and how
>> is disposal being handled
>> 2. Is there an alternative to using paper in the coating booth. The
>> disposal issue will still remain
>>
>> I do not want to put the paper in the UV oven for curing.
>>
>> Any advice will be greatly appreciated.
>>
>> Thanks,
>> Amol
>>
>>
>>
>>
>>
>> WARNING: Export Control
>> This document may contain technical data within the definition of the
>> International Traffic in Arms Regulations (ITAR), and subject to the
>> Export
>> Control Laws of the U.S. Government. Transfer of such data by any
>> means to a
>> foreign person, whether in the United States or abroad, without proper
>> export
>> authorization or other approval from the U.S. Department of State is
>> prohibited.
>>
>> CONFIDENTIALITY NOTICE:
>> This e-mail, and any attachments, is for the sole use of the intended
>> recipient(s) and may contain information that is confidential and
>> protected from disclosure under the law. Any unauthorized review, use,
>> disclosure, or distribution is prohibited. If you are not the intended
>> recipient, please contact the sender by reply e-mail, and delete/destroy
>> all copies of the original message and attachments.
>> Thank you.
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives
>> Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
>> information, or contact Keach Sasamori at [log in to unmask] or
>> 847-615-7100 ext.2815
>> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
> ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|