I am guessing your "cracks" are inner layer separations. This can
happen with or without removal of unused inner lands if the process
used to plate the hole wall is not good.
Can you tell whether the separations are between the electroless
and inner layer, within the electroless or between the electroless
and electrolytic copper plating?
Susan Mansilla
Robisan Lab
################################################################