Would Conformal coating provide better protection... No need to use and
potentially entrap all these corrosive chemicals.
Alain Savard, B.Sc. Chemistry
Chemical Process Analyst
CAE Electronics Ltd.
-----Original Message-----
From: Ralph Richart
Subject: [TN] still confused
We have answers....
So I had a long talk with my customer this morning to provide input
based on the invaluable advice from you all.
I said - "is there a specific reason for choosing 3-8u" of immersion
gold over tin/lead solder?"
He said - "absolutely, the gold provides corrosion resistance, the gold
does not"
I said - "even such a thin amount - only 3-8u"?"
He said - "definitely, all we need is the coverage, the thickness is
irrelevant"
Is this true?
Needless to say, we are rebuilding the parts as we speak. Rework sounds
difficult to say the least, although I may try to come up with some
scheme for fun as they have a bunch of boards that are no good right
now.
thanks for all the help.....
ralph
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|