Subject: | |
From: | |
Date: | 1 Mar 1996 10:46:50 -0800 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Mail*Link(r) SMTP FWD>FAB- (table cleanup) E-GLASS VS. S-GLASS
Technet receipients -- as I read my received copy of the FAB-E-GLASS VS
S-GLASS
I saw a gross formatting problem between what I sent and what I received back
from technet. What I've done is to add underscore place holders (______) in
place of spaces in the table of characteristics. (Off line I'll check to see
where the cockpit problem is, I might have been using a porportional or
variable pitch character font.)
--------------------------------------
Date: 3/1/96 10:27 AM
From: Ralph Hersey
Subject: Time: 9:02 AM
OFFICE MEMO FAB: E-GLASS VS. S-GLASS Date: 3/1/96
Jim Marsico, [log in to unmask], queried about the differences between E-glass
and S-glass fabrics as follows:
The following are some of the properties:
_____________________________ Glass type
__________________|___"E"____|___"S"____|___"D"____|
Tensile, lb/sqin__|___500 k__|__600+ k__|__300+ k__|
TCE ppm/deg F_____|____2.8___|____1.6___|___1.7____|
Dk @ 10 MHz_______|___~6.1___|___~5.2___|____~4____|
Df @ 10 MHz_______|__~0.004__|__~0.007__|__~0.003__|
Ralph Hersey, [log in to unmask]
|
|
|