Several large PCB shops and laminators are using substantial amount of
12 micron copper foil in Japan. They said handling was not easy at the
first
stage, but now nobody is talking about handling difficulty. Experience
solved the problem.
F.Kuwako
Mitsui Mining Smelting Co.
Copper Foil Division
Japan
----------
> 差出人 : James Ying <[log in to unmask]>
> 宛先 : [log in to unmask]
> タイトル : 12 micon copper foil
> 送信日時 : 1997年2月5日 1:31
>
> Is anybody using 12 um thick copper foil in multilayer in big volume ?
> I was told handling is a big question mark. Is this true ?
> Thank you for reply
> James Ying
>
>
***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05
*
>
***************************************************************************
> * To unsubscribe from this list at any time, send a message to:
*
> * [log in to unmask] with <subject: unsubscribe> and no text.
*
>
***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact
*
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]
*
>
***************************************************************************
>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|