Hi Terry -
It's Friday and adhering a nickel plated magnet to PTFE is a Monday
type question! Give Dave Torp at Kester Solder a call - 847-699-5593 -
he is pretty good with goops and glues.
Dave Hillman
Rockwell Collins
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: GEN: Adhesives
Author: [log in to unmask] at ccmgw1
Date: 6/7/96 1:03 PM
Good Day All,
We are looking for someone who is an expert or knowledgable in the realm of
adhesives who would like to consult with us on a project that is giving us
some problems. The application is bonding a nickel plated magnet to a PTFE
base.
If there is anyone interested, please contact:
Terry Munson
Contamination Studies Laboratories
(317) 457-8095.