Ioan,
If you want a polymer selectively gone, Dynaloy is an excellent choice.
Chris
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Monday, November 29, 2010 3:15 PM
To: [log in to unmask]
Subject: Re: [TN] Cleaning of ACF bonder
Steve,
I need to clean boards that were poorly bonded, trying to remove the adhesive residue so that they be bonded again.
Thanks,
Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer T | 450.967.7100 ext.244 E | [log in to unmask] W | www.digico.cc
N'imprimer que si nécessaire - Print only if you must
-----Message d'origine-----
De : Steven Creswick [mailto:[log in to unmask]]
Envoyé : November-29-10 2:29 PM
À : 'TechNet E-Mail Forum'; Ioan Tempea
Objet : RE: [TN] Cleaning of ACF bonder
Ioan,
I am confused.
Are you attempting to clean the ACF bond head, or the substrate, or both?
Steve Creswick
http://www.linkedin.com/in/stevencreswick
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Monday, November 29, 2010 1:32 PM
To: [log in to unmask]
Subject: [TN] Cleaning of ACF bonder
Dear Technos,
We need to clean the ACF bonder from a fair quantity of boards (about 1K/ month). The material to clean is Hitachi Anisolm, per the specification below (unfortunately there's not much in this spec)
http://lituo.testmart.cn/Images/UpLoadForderElse/2009_12_30_13_38_38_4939.pd
f
<http://lituo.testmart.cn/Images/UpLoadForderElse/2009_12_30_13_38_38_4939.p
df>
We have been suggested to use a 48 hour soak in 1-Methyl-2-Pyrrolidinone, followed by an acetone cleaning. It is only the bonding contacts that are immersed in the methyl-pyrr..., but the level of substance is only 2 mm away from an overmolded die-attach. The acetone cleaning is local on the contacts.
First question would be: are the above chemicals OK for this usage? Board is FR4, with gold-plated contacts.
Second question would be: what else could we use to remove the bonder?
Manufacturer seems to recommend Dow Corning OS-20, but we were told by our customers it does not exactly work.
Thanks,
Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer T | 450.967.7100 ext.244 E | [log in to unmask] <mailto:[log in to unmask]> W | www.digico.cc <http://www.digico.cc/>
N'imprimer que si nécessaire - Print only if you must
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|