Two things, when using a no-clean flux you will go through more tips
than you do when using a water soluble. Also, Plato makes tips for
different solder systems such as Hakko, Pace, Metcal, Weller and others.
I have found that Plato's tips last much longer than other tips. I was
told by other engineers that Plato started out as a plating company, and
that is one of the reasons their tips last longer. I don't know if that
is true, but they sure do last longer.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Larry Koens
Sent: Monday, October 17, 2005 8:07 AM
To: [log in to unmask]
Subject: Re: [TN] Solder Stations
Doug,
Surprised on your comment on the tips lasting longer. We have found that
we burn through the JBC tips much more quickly then the Metcal. I do
have to agree that the operators prefer the JBC though.......
Larry
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas O. Pauls
Sent: Monday, October 17, 2005 7:31 AM
To: [log in to unmask]
Subject: Re: [TN] Solder Stations
Well Phil, Metcals are fine if you like burning through tips pretty
quickly. We are changing over to the new JBCs. Operators love em and
the tips last a lot longer.
Doug Pauls
Phillip Bavaro
<phillipbavaro@YA
HOO.COM>
To
Sent by: TechNet [log in to unmask]
<[log in to unmask]>
cc
Subject
10/14/2005 10:37 Re: [TN] Solder Stations
PM
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
Phillip Bavaro
<phillipbavaro@YA
HOO.COM>
Hi Roger,
Metcal....for soldering station selection.
The bean counters won't like it, but your operators will love you for
it.
Just make sure your operators are trained in how to use the equipment
correctly.
Learn how to spot bad tips and how to properly take care of the
equipment.
There are lots of options when it comes to desoldering and hot air
rework stations however.
Hope this helps...
Phil
Darrel Therriault <[log in to unmask]> wrote:
Ditto on the MetCal....DJT
Joel Mearig
Sent by: TechNet
10/14/2005 02:49 PM
Please respond to
TechNet E-Mail Forum ; Please respond to Joel Mearig
To
[log in to unmask]
cc
Subject
Re: [TN] Solder Stations
Roger,
You just opened yourself to a mess of e-mails from sales people who
monitor this forum. I am not such a person.
I really like the Metcal irons. They are more expensive but I feel they
perform better than any other iron. I will catch a lot of flack for the
previous statement but hey, I have an opinion.
Good luck. Joel
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of No Name
Sent: Friday, October 14, 2005 10:25 AM
To: [log in to unmask]
Subject: [TN] Solder Stations
I am looking to establish an electrical/electronic capability. I need
advise on the best solder stations to purchase for a general surface
mount, thru-hole new and rework capability.
I will want a variety of tip sizes, easy to change tips, adjustable
temperatures in some manner, good capacity (little temperature
fluctuation when you put the tip on high mass connections), no current
leakage, and no stray voltages.
Thanks,
Roger
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
Yahoo! Music Unlimited - Access over 1 million songs. Try it free.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|