Scott,
The via size will depend on the pitch of the BGA. Check out sources like
Motorola's End User Manual for BGA
Products (C4PKGUSERGUIDE/D).
I am currently using 25/13 vias for a 50mil pitch BGA. I have also seen
BGA's with a pitch so small that
the via has to be placed on the BGA PAD and filled.
Scott Buscomb
Techsonic Industries, Humminbird Marine Electronics
[log in to unmask]
Scott D. Shepard wrote:
> Hi,
>
> I've done layouts in many types of technologies, but not BGAs. I find
> myself finally needing some tips on the basics. I understand the trace
> pattern to wire up the device, but, how do i figure out whether I can
> use a via, say .02(.5mm) or if I must go to microvia technology. Any
> info will be helpful, ASAP! Were starting a hot project right now.
> Thanks in advance.
>
> Scott
>
> ################################################################
> DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
> To subscribe: SUBSCRIBE DesignerCouncil <your full name>
> To unsubscribe: SIGNOFF DesignerCouncil
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
> ################################################################
################################################################
DesignerCouncil E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE DesignerCouncil <your full name>
To unsubscribe: SIGNOFF DesignerCouncil
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|