Julie,
A quick EDS should be able to pint to the source. It appears the bond wires are
missing, could this be what remains of the wires?
Bhanu
On 10/8/2015 12:21 PM, Julie Silk wrote:
> We had an intermittent failure on a part and after decap, there was a rope-like line that seemed to weave in and out of the circuitry. I'm having Steve Gregory post a picture. I'd like your thoughts on what is going on. We're consulting with the supplier, but I'd like your input.
--
Bhanu Sood
Center for Advanced Life Cycle Engineering (CALCE)
Test Services and Failure Analysis Laboratory
University of Maryland
Room 0128, 4298 Campus Dr. (Bldg. 88)
College Park, MD 20742 USA
Tel: +1 (301) 405 3498
Fax: +1 (301) 314 9269
e-mail: [log in to unmask]
Skype: calce_umd
website: www.calce.umd.edu/TSFA
Confidentiality Notice: The information contained in this e-mail and
any attachments may be legally privileged and confidential. If you are not
an intended recipient, you are hereby notified that any dissemination,
distribution or copying of this e-mail is strictly prohibited.
If you have received this e-mail in error, please notify the sender
and permanently delete the e-mail and any attachments immediately.
You should not retain, copy or use this e-mail or any attachment
for any purpose, nor disclose all or any part of the contents to any
other person.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|