Technet,
Just wanted to say, yes, very few failures have occurred due to voiding,
and the situations I pointed out were extreme situations. But the
interposer attachment failures I described have also happened to others
in not very severe conditions. There is something about interposer
attached parts and voids that do not mix well.
Ioan, I may be mistaken, but I was told that flux entrapped inside of
voids is nothing to worry about because corrosion cannot occur due to a
lack of oxygen. The voids are sealed. Any chemical or metallurgical
engineers out there care to respond to this? I would like to know if
that is true.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Tuesday, October 18, 2005 7:32 AM
To: [log in to unmask]
Subject: Re: [TN] Voids in BGAs, again
Concur with Richard,
good document, professional and academic. But if I am not mistakening,
it does not mention real failures from voiding.
BTW, your experience is very well appreciated, extreme conditions, bad
voids. I am wondering if regular testing, like HALT and the others
caused joints to fail due to voiding.
What about failures due to chemistries, WS flux entrapped into voids
that corrode their way out?
Best regards,
Ioan
> -----Original Message-----
> From: TechNet [SMTP:[log in to unmask]] On Behalf Of Stadem, Richard
> Sent: Tuesday, October 18, 2005 8:14 AM
> To: [log in to unmask]
> Subject: Re: [TN] Voids in BGAs, again
>
> Thank you Steve!
> This is an excellent and informational document. Thank you for posting
> it.
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|