If glass beads are allowable, that maybe your answer....beads are available in
many sizes and they are mixed with your epoxy and then applied....
Marcelo
-----Original Message-----
From: Paul Allen [SMTP:[log in to unmask]]
Sent: Tuesday, May 19, 1998 2:29 PM
To: [log in to unmask]
Subject: [TN] TN Electrical Conductive expoxy use of
Dear Tech Netters,
I have an application requiring the use of AIT electrical conductive
expoxy, ME 8452 does anyone have an experience in controlling thickness
of bond lines.Currently with our application bonding two PCB's together,
squeeze out is proving hard to control. Our customer wants zero. Any
ideas.
Paul Allan.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|