The *breakdown potential gradient* or *dielectric strength* (units: MV/m)
is the electrical potential gradient at which an insulator breaks down and
a damaging surge of current like a lightning strike flows through it. It
is measured by increasing, at a uniform rate, a 60 Hz alternating potential
applied across the faces of a disk of the material in the capacitor-like
configuration of Figure 1 until breakdown occurs, typically at a potential
gradient of between 1 and 100 MV/m. The breakdown potential gradient is a
characteristic property of a dielectric (see *Dielectric constant
(permittivity)<http://inventor.grantadesign.com/en/notes/science/material/S14%20Dielectric%20properties.htm>
*).
Inge
On 25 June 2013 09:43, McGlaughlin, Jeffrey A <[log in to unmask]>wrote:
> Breakdown is measured per IPC-TM-650 2.5.6.3 and is the failure point of
> the dielectric material. Dielectric strength per IPC-T-50 is the maximum
> working condition where breakdown does not occur over a specified time at
> conditions (temp/humidity/pressure.)
>
> Jeffrey McGlaughlin
>
> Engineering Designer
> Tactical Systems Aerospace
> Office (614)424-7582 Fax (614)458-7582
> Battelle 505 King Ave. Columbus, OH 43201
>
>
> This message and any attachments is intended only for the use of the
> individual or entity to which it is addressed, and may
> contain information that is privileged, confidential and/or otherwise
> exempt from disclosure under applicable law. If the reader
> of this message is not the intended recipient or the employee or agent
> responsible for delivering the message to the intended
> recipient, any disclosure, dissemination, distribution, copying or other
> use of this communication or its substance is prohibited.
> If you have received this communication in error, please return to the
> sender and delete from your computer system.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Michael Strong
> Sent: Tuesday, June 25, 2013 12:25 PM
> To: [log in to unmask]
> Subject: [TN] Dielectric Breakdown vs Dielectric Strength
>
> I was reading through a specification sheet and noticed that both
> Dielectric
> breakdown and Dielectric strength were mentioned. Both had the same units
> (V/mil) but the dielectric breakdown was considerably higher. My questions
> are what are the difference between the 2 and how do you measure Dielectric
> breakdown? Thanks
>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|