Hi Victor
I see a misinterpretation of my original question and premise here.
1) we are still in the theoretical area here, we have built boards but not yet underfilled. The BGA joints look perfect in both Ersascope inspection and X-Ray. There are no failing parts.
2) We are about to start shipping product. This product goes into a vehicle, hence the vibration / shock surviveability requirement.
3) what I'm looking for opinions on is simply how much voiding in an underfill material is expected / acceptable.
Given the lack of responses on this question I guess I have to continue my search elsewhere. Ah well, TechNet can't answer everything...
A good day to all.
regards,
Graham Collins
Process Engineer,
Northrop Grumman Canada
Atlantic Facility
(902) 873-2000 ext 6215
>>> <[log in to unmask]> 09/10/02 03:51PM >>>
Graham,
Is the " VIBRATION " test within the expected evaluation or do you have a
" MARGINAL " BGA joint, interface, to begin with. What do cross section of
the failing BGA look like especially the Intermetallic Compound, IMC,
region. Is this region smooth or evidence of some large nodules at 1000x
after copper etchant application. Are the failing BGA at random or
location sensitive. How many REFLOW temperatures did this PCBA received.
BGA are ROBUST interfaces.
victor,
-----Original Message-----
From: Graham Collins [mailto:[log in to unmask]]
Sent: Tuesday, September 10, 2002 11:51 AM
To: [log in to unmask]
Subject: Re: [TN] BGA Under fill
Victor
1) TCE is compatable with the board and bga. Not sure why that would
influence an answer concerning voids...
2) main purpose is to provide support to solder joints (vibration
resistance).
3) I "hope" to fill the entire gap (100% fill) - but realistically some
voids are likely to occur. What % of voids are reasonable and acceptable is
the question.
4&5) Loctite 3568 is applied to 2 sides of the component in accordance with
the manufacturer's instructions, the board and part are preheated to 100C
and following application the cure is 15 minutes at 150C.
regards,
Graham Collins
Process Engineer,
Northrop Grumman Canada
Atlantic Facility
(902) 873-2000 ext 6215
>>> [log in to unmask] 09/10/02 10:17AM >>>
Graham,
Have you considered the thermal properties, TCE, of the Locite 3568
product.
Is this compatible with the TCE of the PCB and device carrier.
What is the main PURPOSE of the proposed UNDER FILL application?
How far into the device carrier to you HOPE to FILL?
Will the LOCITE have to be cured?
Is the PCB Pre Heated?
Victor,
-----Original Message-----
From: Graham Collins [mailto:[log in to unmask]]
Sent: Tuesday, September 10, 2002 6:09 AM
To: [log in to unmask]
Subject: [TN] BGA Underfill
Good day TechNet!
A question for the BGA / Underfill guru's out there (hopefully we have some
of those online).
Using a capillary flow underfill on a BGA, say a .050 pitch 26x26 array,
what is a reasonable result to expect with respect to voiding? Should this
process result in no voids, some voids, lots of voids? Given the size of
this part (1.38" square), is it reasonable to expect a void free underfill?
The particulars: I'm using Loctite 3568 underfill, applied using a syringe
along two edges (L pattern). Product is on a hotplate at 100C.
Thanks all!
regards
Graham Collins
Process Engineer,
Northrop Grumman
Atlantic Facility of Litton Systems Canada
(902) 873-2000 ext 6215
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|