There was a paper presented by Peter Gabriele at a MacDermid Seminar I
attended. He explained quite completely their (MacDermid's) research into
this question. The presentation was entitled "Influence of Solder Mask
Composition on Solder Ball Formation Using No-Clean Flux." You can contact
them at: 203/575-5651.
Ray Rasmussen