TECHNET Archives

May 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Charles Barker <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 8 May 1998 16:07:31 -0500
Content-Type:
multipart/mixed
Parts/Attachments:
text/plain (2306 bytes) , att1.unk (2583 bytes)




Charles Barker@I-O INC
05/08/98 04:07 PM

I believe more and more via's will need to be plugged as more BGAs come
into play.
 I have a lot of concerns about some of the boards we have produced because
of some of these concerns.




Please respond to [log in to unmask]; Please respond to
      [log in to unmask]

To:   [log in to unmask]
cc:    (bcc: Charles Barker/US/I-O INC)
Subject:  Re: [TN] Via Reliability




In General what you everyone say is the amount of Sq. Footage of Boards
that need to be plugged annually?
Russ Smith
Primary Image Specialist
Ciba Specialty Chemicals
 ----------
From: Anderson, Greg (MIS, GEFanuc, NA)
To: [log in to unmask]
Subject: [TN] Via Reliability
Date: Tuesday, May 05, 1998 4:04PM
        There have been numerous postings to this forum over plugging,
capping, and other means of sealing one or both sides of a PWB coated
with
LPISM.  Many PWB vendors use processes where LPISM is applied over bare
copper, then surface finish (HASL, other immersion metallization, or
OSP) is
applied.
        I don't know anyone who offers a 100% guarantee of the integrity
of
the "seal" of the via holes.  If one side of a via has a pin-hole or
crack,
and then is processed through acid cleaners, micro-etches, and
aggressive
fluxes, will these chemicals be drawn in by capillary action, and not
effectively rinsed?  Would a subsequent "capping" operation further seal
these corrosives in place?  It only takes one failed via to cause a
field
failure, or worse, an intermittent.  Is anyone else out there concerned
about this, or is it only one man's unease?
Thanks for your responses,
Greg Anderson
Advanced Manufacturing Engineer
GE Fanuc Automation, N.A.
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################



ATOM RSS1 RSS2