Gerry
Here are the numbers for density of the gold deposit:
Hard gold: density is 17.5 gm/cc (for both Co and Ni hardened gold).
Soft Gold: density is 19.3 gm/cc.
Immersion gold is soft gold or pure gold and hence has a density of 19.3
gm/cc.