Scott
Try 1% monoethanolamine or TEA at 30-45oC
that may help.
Scott B. Westheimer wrote:
> We are using a liquid photo resist and have tried many strippers
> without being able to get a filterable particle size. Either the film
> completely dissolves or comes off in sheets. I am told that this is
> common with this type of film. Any suggestions? Scott
--
Jacob Mozel
11 Hakalanit St
44280 Kfar Saba, Israel
Tel: +972 9 7425871
Fax: +972 9 7424089
e-mail: <[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################