For your first question you can refer to the IPC-TM-650. I'm not going to
repeat it here.
2nd question: If you have a thick laminate/board, use a razer blade or
exaco knife to pick up the edge and pull. If you have a thin laminate or
flex material, put one edge under flame, it will delaminate.
Mason Hu
[log in to unmask]
______________________________ Reply Separator _________________________________
Subject: PWB Fabrication: Copper Peel Strength
Author: [log in to unmask] at corp
Date: 4/11/97 10:22 AM
How does one test for the copper peel strength on standard PWB?
How does one start the peel of the copper so that it can be pulled
with an Instron, etc.?
David Malanchuk (716) 726-4843
Electronic Products
Kodak Equipment Manufacturing Division
Rochester, NY
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|