I forgot to mentioned these tapes are inexpensive, do not have
memory ( stay were put) and take 77 deg C for 20+ hours.
Ramon
-----Original Message-----
From: Dehoyos, Ramon
Sent: Monday, February 05, 2007 9:15 AM
To: 'TechNet E-Mail Forum'
Subject: RE: [TN] Humiseal Masking Tape Residues/latex peelable
Hi Steve:
Another tape, good for masking, is Scotch Y-231 (3M CTR, SAINT
PAUL, MN 55144-1000) or check this site:
http://www.desco.com/DescoCatalog/Packaging/AntistaticTapes/. Note:
when rolling out tape, pull tape out slowly in the presence of deionized
air specially when humidity is low.
Regards,
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, February 05, 2007 8:59 AM
To: [log in to unmask]
Subject: Re: [TN] Humiseal Masking Tape Residues/latex peelable
Hi Steve!
The tape is new, and all the operators that we have in our conformal
coating area have been with the company for quite some time now and are
very familiar with the process. I've stood and stared over peoples
shoulders so much that they've felt self-conscious and think that I
think they've done something wrong, which is the last thing I want to
do. I have one senior operator that I trust as my "second set of eyes",
and he tells me that the process is being carried out as it always has
been. First a pre-bake after final cleaning, then mask, spray, wait 1/2
- 1 hour and then de-mask. The boards aren't baked with the tape on, nor
are they hot from the pre-bake, they are at room temperature when they
are masked.
For the time being, I'm going to have the few areas on the assemblies
that we mask and see the residues, de-masked immediately after spraying
before the coating has a chance to cure at all, and see if that helps
the situation. I'm going to do this until I am able to try the tape that
Amol Kane recommended to me, the 3M Scotch 4737T which I am ordering
today.
I'll let ya'll know how it works out...
-Steve Gregory-
________________________________
From: Steve Mikell [mailto:[log in to unmask]]
Sent: Monday, February 05, 2007 1:11 AM
To: TechNet E-Mail Forum; Steve Gregory
Subject: Re: [TN] Humiseal Masking Tape Residues/latex peelable
Steve
Ok, let's make a complete list of things to check.
The tape... was it an old roll, or a new roll, do you have lot control
on shop supplies and process materials, could this be from a lot not
recently used???
The operator... was this assembly taped by the usual person... did they
notice anything different, warm boards, wet boards, funny smell???
Raw boards... are they from a new lot date code, or new vendor. Do they
look or feel different?
The conformal coating... new batch??, old batch, what about the
thinner, same questions, anything else added to the mix than CC and
thinner.
Did the spray operator change?? did the operator notice anything
different, did anything happen?? did they spray, strip, clean, bake and
spray again, without retaping to save time???
Spray equipment maintenance... did the equipment get cleaned just before
this happened... what kind of cleaning fluids were used???
Pre-masking cleaning... anything happen here, is there a Pre-bake before
masking, or did somebody skip bake or do a post-masking bake... did they
mask warm or hot boards trying to save time...
Have the operators walk you through it, collect all the materials, check
all the other materials in the area. Make sure that you tell the
operators that you are not looking for somebody to pin this on, but you
need to fix the problem. You NEED their help, their ideas, suggestions,
etc...
Also let them know that if they did make a mistake, to tell you, so you
can report back to management that an error was acknowledged, corrected,
and will not happen again. Also remind the operators that when something
goes wrong (like a supervisor telling them to violate procedure to save
time) that they should notify the process engineer ASAP to reduce the
damage. My favorite reason for computer controlled processes is the
reduction of supervisor influence on my processes!!
I repeat, do the walkthrough... its amazing what you will learn.
Steve Mikell
[log in to unmask]
----- Original Message -----
From: "Steve Gregory"
To: [log in to unmask]
Subject: Re: [TN] Humiseal Masking Tape Residues/latex peelable
Date: Fri, 2 Feb 2007 14:18:31 -0600
Hi Michael!
Believe it or not, it is adhesive. When we go to remove the
residue,
it's real gummy and sticky...just like the tape adhesive. Take a
look at
this picture:
http://stevezeva.homestead.com/files/Tape_Adhesive.jpg
It's a piece of the tape that I've taken and carefully scrapped
at on
the sticky (adhesive) side until I've gotten to the carrier part
of the
tape, and the carrier part of the tape is actually clear...it's
the
adhesive that's tan. I looked at the MSDS and the tape is
actually a
polyethyleneterephthalate film, and the adhesive is listed as a
rubber
adhesive.
Like I said, I've never had this problem before.I used Humiseal
tape
over at LaBarge while I was there, and switched our conformal
coat area
over to the tape since I've been here at OAI. I've just now
started
seeing the problem.
The tape doesn't stay on the board for more than 1-hour after
spraying
before we remove it. The one weird thing that I am seeing is
that I only
see the residues at places like in my first picture where we've
masked
over PTH locations where the tape is completely on the PCB
soldermask. I
don't see the residues on places where the tape is over the
tin/lead
board finish, or metal (like the connector sheilds on press-fit
connectors.
-Steve Gregory-
--
<http://a8-asy.a8ww.net/a8-ads/adftrclick?redirectid=en-mail_a_01>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|