We are using a material called "Matrix Moe" supplied by:
Elastomeric Technology Inc.in Hatboro, PA
phone 215-672-0787
fax 215-672-4633
The material consists of oriented gold conductors which are approximately 13
microns by 125 microns. The conductors are embedded in a silicone elastomer
matrix.
_______________________________________________________________________________
Subject: FAB; ASSY: Conductive Elastomer
From: [log in to unmask] at Internet
Date: 7/8/96 6:13 PM
Hello TechNet...
Has anyone ever seen a conductive and machinable elastomer? If so please let
me know a sorce that I can contact. We need such a material for electrical
testing of wirebond pads at a pitch of 175-225 microns.
Any suggestions and tips are welcomed.
Best Regards, Mike Freda
ProLinx Labs
408-227-0707 x105
408-227-6529 (fax)
The mail list is provided by IPC using SmartList v3.05
To unsubscribe from this list at any time, send a message to:
[log in to unmask] with <subject: unsubscribe> and no text.
The mail list is provided by IPC using SmartList v3.05
To unsubscribe from this list at any time, send a message to:
[log in to unmask] with <subject: unsubscribe> and no text.
|
|
|