     The values I have are 6.3 Er for E-glass and 3.6 Er for 
     (Multifunctional) resin.
     
     (Can't answer the S-glass question but I'd like to see the answer.)
     (S-glass is >$$$$$ and available with high temp resin systems. i.e.,
     CE and Poly. It has more favorable CTE values like 9 PPM in X and Y.)
     
     Dave 

______________________________ Reply Separator _________________________________
Subject: Re: FAB: E-GLASS VS. S-GLASS
Author:  [log in to unmask] at SMTPLINK-HADCO
Date:    2/29/96 10:08 PM


Can anyone add to this the Dk for E-glass vs S-Glass?
     
>Can anyone describe the differences in physical properties between E-glass and 
>S-glass cloth?  What resin is typically used with S-glass?
>
>J. Marsico
>AIL Systems, Inc.
>[log in to unmask]
>
>
>
D. Rooke
([log in to unmask])
     
     