Kenny,
A terpene based material dissolving Teflon? Either there is something else
in that material that you should be scared of or someone pulled a fast one
on you with that tape! Personally I don't know of anything that will
dissolve a pure, fully polymerized PTFE, short of maybe boiling aqua regia
or molten sodium hydroxide. I will see if I can get a copy of the MSDS for
Citrex from our local EHS guy.
regards,
Bev Christian
Nortel Networks
> -----Original Message-----
> From: Graham Naisbitt [SMTP:[log in to unmask]]
> Sent: Friday, August 13, 1999 7:09 AM
> To: [log in to unmask]
> Subject: Re: [TN] SILICONE CONTAMINATION & Cooked Latex Mask
>
> Hey Kenny,
>
> This one should be passed to Jim Marsico for his SILICONE problem. If it
> dissolved PTFE it should get rid of the silicone.
>
> Regards,
> Graham Naisbitt
>
> [log in to unmask]
>
> WEB: http://www.concoat.co.uk
>
> CONCOAT Ltd
> Alasan House, Albany Park
> CAMBERLEY GU15 2PL UK
>
> Tel: +44 (0) 1276 691100 Fax: +44 (0) 1276 691227
> ----- Original Message -----
> From: Kenny Bloomquist <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Thursday, August 12, 1999 6:00 PM
> Subject: Re: [TN] Cooked Latex Mask
>
>
> > Graham,
> >
> > I don't know if it will work but we use a product called Citrex, a
> citrus
> > based material, for a lot of different stripping applications. One
> > application is removing dried UR conformal coating from things like
> spray
> > guns. I recently soaked some fittings that had teflon tape left on them
> and
> > it disolved the teflon tape. May be worth a shot but I would keep it
> away
> > from the board material.
> >
> > Ken Bloomquist
> > Sr. Principal Process Engineer
> > PRIMEX Aerospace Company
> > P.O. Box 97009
> > Redmond, WA 98073-9709
> > http://www.primextech.com
> >
> > Ph: 425-885-5000
> > FAX: 425-882-5786
> > [log in to unmask]
> >
> > Northcon/2000, Board Member
> > http://www.northcon.org
> >
> > Electronics Manufacturers Association (EMA), Vice President
> > http://www.ema-wa.org
> >
> > ##############################################################
> > TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> > ##############################################################
> > To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> > the body:
> > To subscribe: SUBSCRIBE TECHNET <your full name>
> > To unsubscribe: SIGNOFF TECHNET
> > ##############################################################
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> > information.
> > If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
> or
> > 847-509-9700 ext.5365
> > ##############################################################
> >
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|