Type II = 99.0 percent Gold minimum
Grade C= Knoop hardness 130-200, incl.
Class 00 = 0.00002 inch thick, minimum
> --Original Message-----
> From: TPE Engineering TechNet [SMTP:[log in to unmask]]
> Sent: Friday, August 27, 1999 10:50 AM
> To: [log in to unmask]
> Subject: [TN] Mil-G-45204
>
> I have a drawing that requires keypads to be plated with
> gold. This drawing references MIL-G-45204, type 2, grade C
> class 00. What type of gold is this? Electrolytic, immersion
> or electroless. How much nickel is required to be plated
> under this gold? Any help I can get on this would be
> appreciated.
> Thanks,
> Ron Hayashi
> Toppan Electronics
> 1-858-695-2222, ext. 243
> [log in to unmask]
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|