Hi everyone,
We are experimenting with  Intrusive reflow (through-hole reflow).  We're
looking for a method to wash boards that are misprinted.  We've tried some
methods but they were unsuccessfull because there is still some solder paste
left in the holes.  Is there a special way, that is used in the industry,
to clean the holes or is there a machine that exist and could solve our problem?

Thanks and have nice day!
Eric Pilon
Tel: (514) 685-7230 x.2586
Fax: (514) 685-3415
QA - Matrox Electronic Systems Ltd.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2